Frit A 3363

Description: Reimbold & Strick cobalt frit

Oxide Analysis Formula Tolerance
B2O3 13.00% 0.83
CaO 3.00% 0.24
ZnO 2.00% 0.11
Na2O 5.00% 0.36
BaO 10.00% 0.29
SiO2 50.00% 3.72
Al2O3 8.00% 0.35
Oxide Weight 406.39
Formula Weight 406.39

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 67 x 10-7 (20-400C)
Frit Softening Point 600C
Glass Transition Temperature 520C
By Tony Hansen