Frit A 4043

Description: Reimbold & Strick high melting frit

Oxide Analysis Formula Tolerance
SiO2 68.00% 2.97
Al2O3 11.00% 0.28
CaO 12.00% 0.56
MgO 5.00% 0.33
K2O 4.00% 0.11
Oxide Weight 262.86
Formula Weight 262.86

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 58 x 10-7 (20-400C)
Frit Softening Point >800C