Crecer Frit 804

Description: Sodium medium borate frit

Oxide Analysis Formula Tolerance
CaO 6.50% 0.31
Na2O 13.05% 0.55
Al2O3 9.30% 0.24
B2O3 11.00% 0.42
SiO2 54.10% 2.37
MgO 0.60% 0.04
K2O 3.60% 0.10
TiO2 0.10% -
Fe2O3 0.28% -
LOI 1.47%n/a
Oxide Weight 259.66
Formula Weight 263.54

Notes

Fusion F43 has a little less KNaO but double the B2O3 and less SiO2. Ferro Frit 3110 is the opposite difference. You could calculate a combination of Frit 3110, Fusion F-43 and Kaolin that would be pretty close to this.

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy