Ferro Frit CC-250-2

Description: Calcium boron source for partially fritted glazes

Oxide Analysis Formula Tolerance
CaO 12.50% 0.64 2.5
K2O 0.50% 0.02 .5
Na2O 7.50% 0.35 2.5
B2O3 17.50% 0.72 2.5
Al2O3 12.50% 0.35 2.5
SiO2 52.50% 2.50 2.5
Oxide Weight 295.05
Formula Weight 295.05

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Hommel Frit 1020
Materials Ferro Frit CC-250
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
Typecodes Available from Laguna Clays

Data

Co-efficient of Linear Expansion 7.73 X 10-6
Frit Softening Point 1500F
By Tony Hansen