Ferro Frit CC-263-2

Description: GLAZE FRIT CONE 04-2

Oxide Analysis Formula Tolerance
CaO 7.50% 0.65 2.5
K2O 2.50% 0.13 2.5
MgO 0.50% 0.06 .5
Na2O 0.50% 0.04 .5
SrO 2.50% 0.12 2.5
ZrO2 0.50% 0.02 .5
B2O3 17.50% 1.23 2.5
Al2O3 12.50% 0.60 2.5
SiO2 52.50% 4.26 2.5
Oxide Weight 471.12
Formula Weight 471.12

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit CC-263
Materials Ferro Frit CC-272
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
Typecodes Available from Laguna Clays

Data

Co-efficient of Linear Expansion 6.79 x 10-6
Frit Softening Point 1850F