1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

No 2 Missouri Flint Clay

Oxide Analysis Formula Tolerance
SiO2 51.20% 2.74 .3
Al2O3 31.70% 1.00 .5
Fe2O3 1.40% 0.03 .3
TiO2 2.00% 0.08 .1
K2O 1.10% 0.04 .4
MgO 0.35% 0.03 .05
CaO 0.80% 0.05 .4
P2O5 0.70% 0.02 .3
Na2O 0.10% 0.01
LOI 13.30%n/a
Oxide Weight 287.50
Formula Weight 331.60

Notes

A semi-plastic Missouri Flint clay. It is well suited for brick and tile manufacturers.

Related Information

Links

Typecodes Fireclay
Fireclays are non-kaolin non-ball clay materials similar to stoneware clays but lacking fluxing oxides. Many fireclays have a PCE of 28 or more.
By Tony Hansen
Follow me on