Degussa Frit 90321

Alternate Names: Zinkbarium fritte

Description: Zinkbarium-fritte

Oxide Analysis Formula Tolerance
ZnO 14.74% 0.40
BaO 27.77% 0.40
PbO 20.21% 0.20
Al2O3 4.62% 0.10
SiO2 32.66% 1.20
Oxide Weight 220.86
Formula Weight 220.86

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 99 x 10-7 (20-400C)
Heating Microscope Analysis for Frits 507C
Heating Microscope Analysis for Frits 770C
Heating Microscope Analysis for Frits 980C