Degussa Frit 90016

Alternate Names: 90016 Alkaliborfritte

Description: Alkaibortntte

Oxide Analysis Formula Tolerance
CaO 7.37% 0.50
B2O3 9.15% 0.50
Na2O 4.07% 0.25
K2O 6.19% 0.25
Al2O3 6.70% 0.25
SiO2 45.81% 2.90
Oxide Weight 301.79
Formula Weight 301.79

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 76 x 10-7 (20-400C)
Heating Microscope Analysis for Frits 564C
Heating Microscope Analysis for Frits 790C
Heating Microscope Analysis for Frits 960C