Greensand

Alternate Names: Glauconite

Oxide Analysis Formula Tolerance
SiO2 100.00% 1.00
Oxide Weight 60.10
Formula Weight 60.10

Notes

A gropu of minerals with a wide range of chemical analyses, having from 2-15% LOI, 35-65% silica, 5-30% alumina, plus CaO (up to 15%), MgO (up to 3.5%), K2O (up to 7%), Na2O (up to 5%).