FinnTalc

Description: Hydrous Magnesium Calcium Silicate

Oxide Analysis Formula Tolerance
MgO 31.00% 1.00
Al2O3 0.20% -
SiO2 61.00% 1.32
FeO 1.90% 0.03
LOI 5.40%n/a
Oxide Weight 122.33
Formula Weight 129.31

Related Information

Links

Materials Talc
A source of MgO for ceramic glazes, a flux or thermal expansion additive in clay bodies, also used in the manufacture of cordierite.
Hazards Talc Hazards Overview
Talc is invaluable in the ceramics industry, it is used as a glaze and body ingredient and as a parting a release agent in various processes. Is it safe?
URLs http://www.mondominerals.com/uploads/tx_drivemondoproducts/FINNTALC_M20SL-AW.pdf
FinnTalc M20SL Data Sheet