Maxum Feldspar

Oxide Analysis Formula Tolerance
CaO 1.45% 0.15
Na2O 6.49% 0.59
K2O 4.41% 0.26
Al2O3 18.10% 1.00
SiO2 67.90% 6.37
Fe2O3 0.50% 0.02
LOI 0.20%n/a
Oxide Weight 557.41
Formula Weight 558.52

Notes

The Unispar trade name is reserved for paint, coatings and functional filler applications.