Feldspar A-300

Description: A-300 BANGALORE FELDSPAR

Oxide Analysis Formula Tolerance
K2O 12.48% 0.73
Na2O 3.01% 0.27
Al2O3 19.06% 1.03
SiO2 64.37% 5.92
Fe2O3 0.19% 0.01
LOI 0.89%n/a
Oxide Weight 547.47
Formula Weight 552.39

Notes

Mined and processed in India to sizes down to 800 mesh (4 micron).
Chemical analysis has been supplied by Essen & Co Assayers, Bangalore, India.

Related Information

Links

Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.