Ceradel Frit 3110

Alternate Names: Ceradel Fritte 3110

Description: High sodium, low boron/alumina frit

Oxide Analysis Formula Tolerance
CaO 6.50% 0.30
K2O 2.50% 0.07
Na2O 15.50% 0.64
B2O3 2.50% 0.09
Al2O3 4.00% 0.10
SiO2 69.00% 2.93
Oxide Weight 254.84
Formula Weight 254.84

Notes

Ceradel provides a slightly different chemistry for this than Ferro does for its 3110 standard formulation.

Related Information

Links

Materials Ferro Frit 3110
High sodium, high thermal expansion low boron frit. A super-feldspar in clay bodies. Melts a very low temperatures.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 100.8 (10-7/C 20/300C)
Frit Melting Range (C) 1000-1300C
By Tony Hansen