Ceradel Frit C 1253

Alternate Names: Fritte C1253, Fritte C 1253, Ceradel Frit 1253

Description: High expansion frit, Fritte boro-alcaline sans plomb

Oxide Analysis Formula Tolerance
BaO 2.54% 0.05 10
B2O3 21.72% 0.95 10
Al2O3 6.43% 0.19 15
Na2O 13.37% 0.66 3
CaO 3.91% 0.21 .5
ZnO 2.16% 0.08
SiO2 49.86% 2.53
Oxide Weight 304.43
Formula Weight 304.43

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.

Data

Co-efficient of Linear Expansion 99x10-7 (20/300C)
Frit Softening Point 880-920C
By Tony Hansen