Feldspar Las Bocas (Cuba)

Description: Cuban feldspar

Oxide Analysis Formula Tolerance
SiO2 72.57% 8.47
Al2O3 15.47% 1.06
TiO2 0.12% 0.01
CaO 1.31% 0.16
MgO 0.69% 0.12
K2O 2.71% 0.20
Na2O 4.55% 0.51
Fe2O3 0.61% 0.03
1.00% -
LOI 1.25%n/a
Oxide Weight 687.31