1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

G20 HP Feldspar

Oxide Analysis Formula Tolerance
CaO 0.75% 0.08
K2O 13.20% 0.79
Na2O 1.52% 0.14
Al2O3 18.20% 1.00
SiO2 65.90% 6.16
Fe2O3 0.09% -
LOI 0.16%n/a
Oxide Weight 559.85
Formula Weight 560.75

Notes

Same chemistry as G200HP.