Fusion Frit F-490C

Description: Strontium frit

Oxide Analysis Formula Tolerance
CaO 9.00% 0.53
K2O 3.50% 0.12
Na2O 2.00% 0.11
SrO 7.60% 0.24
Al2O3 10.30% 0.33
B2O3 12.40% 0.59
SiO2 55.20% 3.03
Oxide Weight 329.82
Formula Weight 329.82