Fusion Frit FZ-81

Description: Mystery frit without exact chemistry

Oxide Analysis Formula Tolerance
Li2O 2.50% 0.26 .5
Na2O 6.50% 0.32 2.5
K2O 2.50% 0.08 1.5
CaO 4.50% 0.24 1.5
ZnO 1.50% 0.06 1.5
SrO 1.50% 0.04 1.5
Al2O3 12.50% 0.37 2.5
B2O3 12.50% 0.55 2.5
SiO2 55.00% 2.79 5
Oxide Weight 301.47
Formula Weight 301.47

Notes

We only have ranges for the chemistry on this material.

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 8.2
Frit Softening Point 1350C