| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| K2O | 0.03% | 0.02 | |
| Na2O | 0.07% | 0.09 | |
| CaO | 0.51% | 0.69 | |
| MgO | 0.11% | 0.21 | |
| Fe2O3 | 0.07% | 0.03 | |
| Al2O3 | 0.18% | 0.13 | |
| SiO2 | 99.03% | 124.19 | |
| LOI | 0.16% | n/a | |
| Oxide Weight | 7,536.96 | ||
| Formula Weight | 7,549.04 | ||
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk