Cendre d\'os

Oxide Analysis Formula Tolerance
K2O 0.03% -
Na2O 0.92% 0.01
CaO 53.70% 0.75
MgO 1.07% 0.02
P2O5 40.10% 0.22
Al2O3 0.05% -
SiO2 0.23% -
LOI 3.11%n/a
SO4 0.00%n/a
Oxide Weight 74.99
Formula Weight 77.40