Cendre de lavande

Oxide Analysis Formula Tolerance
K2O 14.71% 0.18
Na2O 0.39% 0.01
CaO 29.26% 0.61
MgO 5.66% 0.16
TiO2 0.21% -
P2O5 4.88% 0.04
Fe2O3 1.26% 0.01
Al2O3 3.54% 0.04
SiO2 16.59% 0.32
LOI 0.00%n/a
Oxide Weight 89.07
Formula Weight 111.76