Cendre de bois dur ou de chĂȘne

Oxide Analysis Formula Tolerance
K2O 4.04% 0.05
Na2O 0.50% 0.01
CaO 39.67% 0.86
MgO 2.31% 0.07
TiO2 0.19% -
P2O5 1.28% 0.01
Fe2O3 0.94% 0.01
Al2O3 2.09% 0.02
SiO2 29.20% 0.59
LOI 29.20%n/a
Oxide Weight 97.30
Formula Weight 137.44