Ferro Frit 4101

Alternate Names: Formerly Ferro Frit 530

Description: High expansion sodium borosilicate fluorine frit

Oxide Analysis Formula Tolerance
CaO 1.90% 0.08
K2O 20.35% 0.50
Na2O 11.05% 0.42
F 4.35% 0.53
Al2O3 7.22% 0.17
B2O3 11.18% 0.38
SiO2 43.95% 1.71
Oxide Weight 233.58
Formula Weight 233.58

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 530
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
By Tony Hansen