Forshammer Feldspar

Description: Swedish feldspar

Oxide Analysis Formula Tolerance
SiO2 75.60% 10.31
Al2O3 14.50% 1.17
Na2O 4.80% 0.63
K2O 4.20% 0.37
Fe2O3 0.14% 0.01
LOI 0.60%n/a
Oxide Weight 813.41
Formula Weight 818.32