FFF Feldspar

Alternate Names: FFF K6 Feldspar

Description: Finnish Potash feldspar

Oxide Analysis Formula Tolerance
SiO2 66.30% 7.14
Fe2O3 0.10% -
Na2O 5.50% 0.57
Al2O3 18.60% 1.18
K2O 6.20% 0.43
SO4 0.30%n/a
Oxide Weight 625.78
Formula Weight 627.66