Soda Feldspar Z-507-P2

Oxide Analysis Formula Tolerance
CaO 0.97% 0.09
MgO 0.26% 0.04
K2O 0.16% 0.01
Na2O 9.83% 0.86
TiO2 0.03% -
Al2O3 19.57% 1.04
SiO2 68.68% 6.21
Fe2O3 0.07% -
LOI 0.43%n/a
Oxide Weight 541.17
Formula Weight 543.51

Notes

A New Zealand material.

Related Information

Links

Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.