Pyrophyllite PPRG53

Oxide Analysis Formula Tolerance
K2O 1.00% 0.07
Na2O 0.10% 0.01
TiO2 0.20% 0.02
Al2O3 15.80% 1.00
SiO2 79.40% 8.53
Fe2O3 0.40% 0.02
LOI 3.10%n/a
Oxide Weight 625.56
Formula Weight 645.57

Related Information

Links

Typecodes Aluminum Silicate
Materials not classifiable as commonly known aluminum silicates. For example, kaolin is a common aluminum silicate.