1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Pot Spar B-801P2

Oxide Analysis Formula Tolerance
CaO 0.01% -
MgO 0.17% 0.02
K2O 10.34% 0.62
Na2O 3.95% 0.36
TiO2 0.01% -
Al2O3 17.58% 0.97
SiO2 65.29% 6.11
Fe2O3 0.07% -
LOI 0.36%n/a
Oxide Weight 547.69
Formula Weight 549.67

Notes

A New Zealand material.