1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Opeal OP-2

Oxide Analysis Formula Tolerance
CaO 0.07% -
MgO 0.10% 0.01
K2O 1.17% 0.04
Na2O 0.10% -
TiO2 0.22% 0.01
Al2O3 33.45% 1.00
SiO2 51.49% 2.61
Fe2O3 0.60% 0.01
LOI 12.80%n/a
Oxide Weight 265.90
Formula Weight 304.93

Notes

A New Zealand material.