Degussa Frit 15098

Description: Frit used in crystalline glazes

Oxide Analysis Formula Tolerance
K2O 10.60% 0.35
CaO 5.05% 0.28
ZnO 7.33% 0.28
Li2O 0.86% 0.09
Al2O3 11.48% 0.35
SiO2 61.09% 3.16
B2O3 3.58% 0.16
Oxide Weight 311.06
Formula Weight 311.06

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.