March 2026: We are doing major upgrades to code here, please be patient regarding any issues. If any page is not working for a period of hours, please contact us. Thank you.

Monthly Tech-Tip from Tony Hansen SignUpFeb 14-15, 2026 - Major Server Upgrade Done

No tracking! No ads!

1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Matrix Frit B70-A

Description: High boron zero silicate calcia alumina frit

Oxide Analysis Formula Tolerance
B2O3 70.00% 4.27
Al2O3 24.00% 1.00
CaO 4.00% 0.30
Oxide Weight 416.50
Formula Weight 416.50

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
Materials Matrix Frit B40-C
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy