Potclays Frit 2266

Alternate Names: Potclays Ferro Crystal Frit

Description: This is actually Ferro Frit 3110

Oxide Analysis Formula Tolerance
CaO 6.30% 0.29
K2O 2.30% 0.06
Na2O 15.30% 0.64
B2O3 2.60% 0.10
Al2O3 3.70% 0.09
SiO2 69.80% 3.03
Oxide Weight 260.76
Formula Weight 260.76

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 3110
High sodium, high thermal expansion low boron frit. A super-feldspar in clay bodies. Melts a very low temperatures.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
By Tony Hansen