Potclays Frit 2265

Alternate Names: Potclays H.T. Borax Frit

Oxide Analysis Formula Tolerance
K2O 1.28% 0.03
Na2O 8.44% 0.33
CaO 14.68% 0.63
MgO 0.05% -
Al2O3 8.91% 0.21
SiO2 48.55% 1.96
B2O3 18.09% 0.63
Oxide Weight 242.35
Formula Weight 242.35

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials PotteryCrafts Frit P2953
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.