1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Elfusa Mullite MUB-S

Oxide Analysis Formula Tolerance
CaO 0.14% -
K2O 0.07% -
MgO 0.18% 0.01
Na2O 0.60% 0.01
TiO2 0.03% -
Al2O3 71.99% 1.00
SiO2 26.60% 0.63
Fe2O3 0.38% -
Oxide Weight 141.67
Formula Weight 141.67