| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.12% | - | |
| K2O | 0.03% | - | |
| MgO | 0.04% | - | |
| Na2O | 0.41% | 0.01 | |
| TiO2 | 0.01% | - | |
| Al2O3 | 72.23% | 1.00 | |
| SiO2 | 27.00% | 0.63 | |
| Fe2O3 | 0.16% | - | |
| Oxide Weight | 141.22 | ||
| Formula Weight | 141.22 | ||