| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 31.30% | 0.99 | |
| K2O | 0.03% | - | |
| MgO | 0.08% | - | |
| Na2O | 0.17% | - | |
| TiO2 | 0.05% | - | |
| ZrO | 67.46% | 1.12 | |
| Al2O3 | 0.42% | 0.01 | |
| SiO2 | 0.23% | 0.01 | |
| Fe2O3 | 0.27% | - | |
| Oxide Weight | 177.64 | ||
| Formula Weight | 177.64 | ||