1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Elfusa Alumina

Oxide Analysis Formula Tolerance
K2O 0.03% -
MgO 0.04% -
Na2O 0.50% 0.01
Al2O3 99.27% 1.00
SiO2 0.08% -
Fe2O3 0.08% -
Oxide Weight 102.75
Formula Weight 102.75