Barium Oxide-Alumina-Silica Eutectic

Oxide Analysis Formula Tolerance
BaO 35.00% 1.00
Al2O3 10.00% 0.43
SiO2 55.00% 4.01
Oxide Weight 438.00
Formula Weight 438.00

Notes

One person questioned these numbers, citing an alternate source claiming 60% SiO2, 10% Al2O3, 30% BaO.

Related Information

Links

Materials Eutectics
Typecodes Eutectic
These are theoretical mixtures of oxides, not real materials. Use these to learn about low melting chemistries.

Data

Frit Softening Point 1200C