Hommel Frit 446

Description: Leadless zinc high boron frit

Oxide Analysis Formula Tolerance
CaO 4.35% 0.18
Na2O 10.66% 0.40
ZnO 14.82% 0.42
B2O3 28.73% 0.96
SiO2 41.44% 1.60
Oxide Weight 231.73
Formula Weight 231.73

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 3824
Materials Pemco Frit P-1733
Materials General Frit GF-100
Materials Fusion Frit FZ-16
The champion in our frit melt-off competitition. This frit showcases the amazing fluxing power of boron and zinc working together. It is 15.5% ZnO.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.