Hommel Frit 378

Oxide Analysis Formula Tolerance
K2O 6.74% 0.19
Na2O 8.74% 0.37
CaO 9.60% 0.45
Al2O3 9.82% 0.25
B2O3 15.75% 0.59
SiO2 49.37% 2.14
Oxide Weight 260.71
Formula Weight 260.71

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 3270
Materials Pemco Frit P-802
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 9.4 x 10-6
Frit Melting Range (C) 1790F