Hommel Frit 576

Description: Calcium borosilicate very low lead frit

Oxide Analysis Formula Tolerance
K2O 1.10% 0.06
Na2O 2.81% 0.23
CaO 6.92% 0.63
PbO 3.49% 0.08
Al2O3 5.61% 0.28
B2O3 24.21% 1.77
SiO2 55.86% 4.74
Oxide Weight 510.24
Formula Weight 510.24

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 3451
Materials Pemco Frit Pb-674
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 5.4 x 10-6
Frit Softening Point 1465F
By Tony Hansen