Ceraflux

Alternate Names: Lead alumina bisilicate

Description: Lead alumina bilsilicate frit (1% alumina)

Oxide Analysis Formula Tolerance
PbO 65.00% 1.00
SiO2 34.00% 1.94
Al2O3 1.00% 0.03
Oxide Weight 343.38
Formula Weight 343.38

Related Information

Links

Materials Lead Bisilicate Frit
A standard frit of 1 molar part of PbO and 2 of SiO2. It is considered stable and non-leachable.
Materials Ceraflux
An alumina lead bisilicate from Hammond Lead Products in Indiana. The data sheet claims it is safe and insoluble in stomach acid.
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.

Data

Density (Specific Gravity) 4.6-4.65
Frit Melting Range (C) 788-816C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy