Hommel Frit 183

Oxide Analysis Formula Tolerance
K2O 1.82% 0.05
Na2O 1.61% 0.06
CaO 17.88% 0.78
PbO 9.81% 0.11
Al2O3 3.54% 0.09
B2O3 19.41% 0.68
SiO2 45.92% 1.87
Oxide Weight 245.10
Formula Weight 245.10

Related Information

Links

Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 7.3 x 10-6 (50-450C)
Frit Softening Point 1800F