Fusion Frit FZ-576

Alternate Names: Fusion Frit FZ576

Description: Ca-Zn transparent monoporosa frit

Oxide Analysis Formula Tolerance
ZnO 11.80% 0.34
CaO 10.00% 0.42
Na2O 5.00% 0.19
K2O 2.10% 0.05
Al2O3 5.80% 0.13
B2O3 4.30% 0.14
SiO2 61.00% 2.38
Oxide Weight 234.66
Formula Weight 234.66

Related Information

Links

URLs http://www.fusionceramics.com/
Fusion Ceramics Frit Website
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 6.2 x 10-6
Frit Softening Point 1800F
By Tony Hansen