Fusion Frit F-582

Alternate Names: Fusion Frit F582

Description: Lithium low fire clear frit

Oxide Analysis Formula Tolerance
Li2O 3.50% 0.34
K2O 2.50% 0.08
Na2O 6.00% 0.28
CaO 5.70% 0.30
Al2O3 7.20% 0.21
B2O3 15.60% 0.65
SiO2 59.50% 2.89
Oxide Weight 292.08
Formula Weight 292.08

Related Information

Links

URLs http://www.fusionceramics.com/
Fusion Ceramics Frit Website
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 8.5 x 10-6
Frit Softening Point 1400F