Fusion Frit F-567

Alternate Names: Fusion Frit F567

Description: Alkali boron frit

Oxide Analysis Formula Tolerance
K2O 5.61% 0.22
Na2O 12.95% 0.77
CaO 0.24% 0.02
Al2O3 11.41% 0.41
B2O3 24.01% 1.27
SiO2 45.78% 2.79
Oxide Weight 366.70
Formula Weight 366.70

Related Information

Links

URLs http://www.fusionceramics.com/
Fusion Ceramics Frit Website
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 9.14 x 10-6
Frit Softening Point 1450F