1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Fusion Frit F-562

Alternate Names: Fusion Frit F562

Description: Alkali boron frit

Oxide Analysis Formula Tolerance
K2O 3.60% 0.16
Na2O 12.26% 0.83
CaO 0.16% 0.01
Al2O3 17.05% 0.70
B2O3 29.83% 1.79
SiO2 37.09% 2.58
Oxide Weight 418.70
Formula Weight 418.70

Related Information

Links

URLs http://www.fusionceramics.com/
Fusion Ceramics Frit Website
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 9.06 x 10-6
Frit Melting Range (C) 1450F
By Tony Hansen