Kernick Kaolin

Description: English kaolin

Oxide Analysis Formula Tolerance
SiO2 48.00% 2.20
Al2O3 37.00% 1.00
Fe2O3 1.00% 0.02
TiO2 0.07% -
CaO 0.06% -
MgO 0.28% 0.02
K2O 2.30% 0.07
Na2O 0.10% -
LOI 11.80%n/a
Oxide Weight 244.83
Formula Weight 277.58

Related Information

Links

Minerals Mica
See Muscovite.
Minerals Kaolinite
The most fundamental clay mineral. This mineral is found in nature in its purest form as kaolin. How
Materials Kaolin
The purest of all clays in nature. Kaolins are used in porcelains and stonewares to impart whiteness, in glazes to supply Al2O3 and to suspend slurries.
Typecodes Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy