D Feldspar

Oxide Analysis Formula Tolerance
CaO 0.39% 0.04
K2O 2.70% 0.16
MgO 0.03% -
Na2O 8.68% 0.79
TiO2 0.03% -
Al2O3 18.71% 1.04
SiO2 68.66% 6.48
Fe2O3 0.17% 0.01
LOI 0.64%n/a
Oxide Weight 563.45
Formula Weight 567.08