Cyprucast

Oxide Analysis Formula Tolerance
CaO 0.06% -
K2O 0.06% -
MgO 0.12% 0.01
Na2O 0.14% 0.01
TiO2 1.55% 0.05
Al2O3 38.25% 1.00
SiO2 45.75% 2.03
Fe2O3 0.41% 0.01
LOI 13.66%n/a
Oxide Weight 230.24
Formula Weight 266.67

Related Information

Links

Typecodes Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content.